Slate Collection Natural Stone
Roll over to zoom product
Indian Multicolor (Brick-joint Natural Cleft) S771
Origin: India
Notes:
- Consult your Daltile Architectural Representative for more information on special sizes. Some finishes may require extended lead times.
- All slab material shown is not necessarily available in all areas.
| Country of Origin | India | |
| Durability | 1 | Residental - Suitable for residential use. Not Recommended for commercial areas. |
| Soundness | Group C | These stones may contain holes, voids, lines or separation and structural flaws. It is standard practice to repair these stones by filling them or reinforcing them. |
| Shade Variation | R | Random: Variegated in color and veining. Blending allowances during installation are strongly recommended. |
| Exterior Usage | EW | Suitable for covered exterior walls in freezing and non-freezing climates. |
| Commercial Exterior Usage | EW | Suitable for covered exterior walls in freezing and non-freezing climates. |
| Stock Tile Sizes And Finishes | 1 1/4" x 2 7/8" x 3/8" (11 3/4" x 11 7/8" sheet) | |
| Stock Slab Sizes And Finishes | N/A | |
| Special Order Sizes Available | N/A | |
| Cut-To-Size Available | N/A | |
| Alternate Finishes Available By Special Order | N/A |
| ASTM Test Method | Value * | * Technical values supplied by the Marble Institute of America (MIA) and American Society for Testing and Materials (ASTM); and provide a frame of reference only. Actual performance may vary. | |
| Absorption by Weight, % | C97 | ||
| Density, lbs./ft | C97 | ||
| Compressive Strength, psi | C170 | ||
| Abrasion Resistance, hardness | C241 | ||
| Flexural Strength, psi | C880 | ||
| Weather Resistance | C217 | ||
| Modules of Rupture, psi | C120 |
| Can be used in interior wet areas, if sealed and maintained properly. If not properly maintained, the stone look could be altered. Please contact your sealer manufacturer or your Daltile sales representative for information about products that can protect the stone from moisture exposure. | |
| A sealer is recommended. (Note: Some limestone and tumbled stone should be sealed prior to grouting.) | |
| These stones caontain deposits or minerals and iron that may react to moisture. Stone bleeding or rusting is a common example of this. These stones should not be used in installations where they would be exposed to standing, run off water or too much humidity. A sealer is stronly recommended but will not prevent the chemical reaction from happening. Please contact your sealer manufacturer for information about products that can protect the stone from moisture exposure. | |
| White thin-set or mortar is recommended. |
DOWNLOADS