| Durability | 1 | Residental - Suitable for residential use. Not Recommended for commercial areas. |
| Soundness | Group A | Sound Stones with no geological voids or fissures. These stones do not require any filling or patching. |
| Shade Variation | M | Medium: Background color contains slight variations. |
| Exterior Usage | N/A | Not recommended for exterior applications. |
| Commercial Exterior Usage | N/A | Not recommended for exterior applications. |
| Stock Tile Sizes And Finishes | 24"x24"x1/2", 12"x24"x1/2", 18"x18"x1/2" & 12"x12"x3/8" Honed | |
| Stock Slab Sizes And Finishes | N/A | |
| Special Order Sizes Available | Yes | Consult your Daltile Architectural Representative for more information on special sizes. |
| Cut-To-Size Available | N/A | |
| Alternate Finishes Available By Special Order | N/A |
| ASTM Test Method | Value * | * Technical values supplied by the Marble Institute of America (MIA) and American Society for Testing and Materials (ASTM); and provide a frame of reference only. Actual performance may vary. | |
| Absorption by Weight, % | C97 | 2.64 | |
| Density, lbs./ft | C97 | 174.19 lbs/ft3 (kg/m3) | |
| Compressive Strength, psi | C170 | 11046 psi | |
| Abrasion Resistance, hardness | C241 | 3.3 | |
| Flexural Strength, psi | C880 | 2,246 | |
| Weather Resistance | C217 | ||
| Modules of Rupture, psi | C120 |
| Can be used in interior wet areas, if sealed and maintained properly. If not properly maintained, the stone look could be altered. Please contact your sealer manufacturer or your Daltile sales representative for information about products that can protect the stone from moisture exposure. | |
| Might contain dry seams, pits, fossils, and glass veins that are filled at the factory or during installation. These are all inherent characteristics of the stone. Since these voids can sometimes lose their fillings, they should be refilled as part of normal maintenance. | |
| A sealer is recommended. (Note: Some limestone and tumbled stone should be sealed prior to grouting.) | |